What are the disadvantages of Gabbeh?

Overgrowth: Overgrowth or so-called elongation and stretching to the length that causes this defect due to insufficient tapping during weaving and improper cream and warp and weft in it.
Downsizing: Downsizing or so-called slang is the shortening of the length of the gabbeh, which causes this defect due to the inadequacy of the cream and the fabric in it.
Interference: If the weaving is not done well or a few rows are not woven during Gabbeh weaving, it will cause the two flowers that are in the symmetrical design not to be woven in the same and symmetrical pattern and the design will not work well.
Emptiness: This defect occurs when the weaver weaves a thick layer of cream and yarn to save on material consumption, which causes hollow or so-called hollow Gabbeh.
Solitude weaving: In other words, it is called simple weaving in which the weaver does not implement some parts of Gabbeh design on Gabbeh according to the plan for ease or lack of accuracy and skill and removes them.
Complexity: The weaver must be careful and skilled in weaving, and weaving must be done after each row of weaving, and the weaves must be well beaten and laid by the weaver. If the pounding is not uniform and principled, complexity arises, so that it causes inconsistency in the ridges, so that one side is the width of the upper Gabbeh and the other side is the lower width, and the edges of the Gabbeh become tubular, which cannot be corrected after the texture is finished.
A multi-fabric fold: Sometimes, in order to save time and material consumption, after weaving each ridge, more weaves are used in each ridge than Gabbeh, which reduces the durability and quality of Gabbeh. And the more fabrics in each Gabbeh ridge, the lower the quality and durability of Gabbeh.
To have bergamot: bergamot or middle plan of Gabbeh in which all the angles of Gabbeh are equal and the same point, provided that Gabbeh’s map is elastic and bergamoted or only bergamoted if all aspects of the texture are not uniformly coordinated during Gabbeh And if the bergamot is not in the middle of the tissue, there will be a problem of bergamot in Gabbeh.
Chewing: Barbing that occurs in the carpet due to lack of care and accuracy in scissors or that the scissors are not sharp and unhealthy.
Two colors: Due to the lack of facilities or not buying wool and cream together and buying different materials several times, it causes Gabbeh duplicity. Also, two colors are created due to the lack of quality and uniformity of the wool, which did not have fixed dyeing properties, or the dyeing on the wool was not done well.
Becoming corny or falling asleep: Paying and cutting too much flesh with scissors is called becoming corned and falling asleep, which is also known as becoming less meaty.
Discoloration: A defect in the form of thin lines on the surface and back of Gabbeh or darker that is completely inconsistent with other parts of the text or behind Gabbeh due to lack of cream and bad dyeing, which means that when dyeing cream, the brain It is not well painted.
Headband: If we fold the gabbeh from the longitudinal part on top of each other so that the transverse parts are not on top of each other, there is a problem with the headband, which is due to the excessive stiffness of the wefts and the lack of precision and skill of the weaver.
Having a shoulder: If the length of one side of Gabbeh is shorter or longer than the other side, this defect is called Gabbeh having a shoulder.
Loosening of the strands: If the Gabbeh tissue lasts longer than usual, due to natural factors such as heat, cold and humidity, the strands will loosen over time and their strength and durability will decrease, and rot may occur in the strands and blows may occur. Tear the cheeks. If we tie the torn knots, after washing the knots, it will appear, which is one of the disadvantages of Gabbeh.
Gabbeh Slate or Gabbeh: Gabbeh usually has different sizes. Among the standard dimensions of Gabbeh are: Gabbeh Zara and Charak, Gabbeh Zare and Nim, Gabbeh Pardehi, Gabbeh Blanket, 3.2, 3.5 / 2.5 / 2, 4.3 , Named 6.4, which is the most finely woven type of blanket. If standard sizes are not used in Gabbeh tissue, the term Gabbeh is called ugly. Fabrics that are standard in size are usually preferred by the customer, unless the customer suggests a size to weave without considering the standard.
Puncture: If the weaver reduces the number of layers of weft in a part of Gabbeh weave or knocks Dafah more firmly than other parts of Gabbeh, in this part more puncture is seen than other parts, which is called beating.
Crooked: This defect may be due to excessive pounding of the first weave of the weave, and with non-uniform wefts or improper finishing work such as lowering and salting, etc., which reduces the quality and value of Gabbeh.
Cyst: A cyst or cyst is a defect that occurs due to the looseness or loosening of the ridges on one side of the gill relative to the other side.
Plain floor: If Gabbeh text is not full in terms of design and only one color is used in it, this term is called Gabbeh plain floor.
Peeling: If one of the four corners of Gabbeh is different from the other corners, Gabbeh has Luchi. This defect is due to excessive loosening of the wefts or inaccuracy of the weaver when cutting and separating the gabbeh from the gallows or when lowering the gabbeh.
In addition to the defects mentioned and the cause of its occurrence should be sought from the stage of preparing materials and tools and how to weave and weave and select the map, after completing the above steps, there may be defects in the next stages of work on Gabbeh. , Including in the stage of washing Gabbeh, hanging, drying Gabbeh in the sun and using various drugs to wash Gabbeh and face and Gabbeh payment.